Insulation Mullite bricks is widely used as insulation materials in high temperature from 1200℃ to 1600℃. It has low thermal conductivity and high strengthen.
Insulation Mullite bricks is widely used as insulation materials in high temperature from 1200℃ to 1600℃. It has low thermal conductivity and high strengthen.



| ITEM | CODE | |||||
| G-23 | G-26 | G-28 | G-30 | G-32 | ||
| SERVICE TEMP.℃ | 1260 | 1430 | 1540 | 1560 | 1600 | |
| BD g/cm3 | 0.5 | 0.8 | 0.95 | 1.05 | 1.1 | |
| MOR Mpa ≥ | 0.7 | 1.1 | 1.6 | 2 | 2 | |
| CCS Mpa ≥ | 1 | 2 | 2.3 | 2.7 | 2.7 | |
| PLC ≤ | % | 0.3 | 0.4 | 0.5 | 0.6 | 0.8 |
| ℃×h | 1230×24 | 1400×24 | 1510×24 | 1530×24 | 1570×24 | |
| THERMAL EXPANSION | 0.5 | 0.6 | 0.8 | 0.8 | 0.8 | |
| RATE 1090℃%≤ | ||||||
| THERMAL CONDUCTIVITY , w/m.k≤ | 400℃ | 0.15 | 0.28 | 0.33 | 0.41 | 0.43 |
| 600℃ | 0.17 | 0.31 | 0.36 | 0.43 | 0.44 | |
| 800℃ | 0.19 | 0.33 | 0.39 | 0.45 | 0.52 | |
| 1000℃ | 0.24 | 0.35 | 0.42 | 0.48 | 0.55 | |
| AL2O3%≥ | 37 | 50 | 60 | 68 | 72 | |
| Fe2O3%≤ | 1 | 1 | 0.7 | 0.5 | 0.5 | |
| SiO2%≤ | 45 | 43 | 36 | 29 | 25 | |